Sign In | Join Free | My insurersguide.com
China Suzhou Xunshi New Material Co., Ltd logo
Suzhou Xunshi New Material Co., Ltd
SUZHOU XUNSHI NEW MATERIAL CO., LTD CHOOSE XUNSHI, CHOOSE HIGH PERFORMANCE
Verified Supplier

8 Years

Home > Inconel Nickel Alloy >

Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy

Suzhou Xunshi New Material Co., Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy

Brand Name : XUNSHI

Model Number : N07818

Certification : ISO9001:2015

Place of Origin : China

MOQ : 200kg

Price : Negotiable

Payment Terms : T/T

Supply Ability : 5000kg per month

Delivery Time : 45-60 days

Packaging Details : Plywood case

UNS no. : N07818

Equal name : ATI 718Plus, Allvac 718Plus

Spec : AMS 5441, AMS 5442

Avialable forms : ingot, billet, block, forged round bar, hot-rolled shapes and rectangles, bar, rod, wire, plate, sheet, strip, and castings.

Density : 8.25g/cm

Contact Now

Inconel 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the high temperature capability and thermal stability of Waspaloy alloy while retaining the processing characteristics of 718 alloy. It is double vacuum melted (VIM/ESR/VAR). This VIM/VAR process ensures excellent microcleanliness and tight compositional control. Triple melting, with electroslag remelting between the VIM and VAR operations, minimizes the possibility of macrosegregation, increases microcleanliness, and is preferred for premium quality jet engine rotating component applications. Inconel 718Plus alloy has at least a 100°F (55°C) operating temperature advantage over 718 alloy. 718Plus alloy also has advantages over Waspaloy and other higher temperature capable, nickel-base alloys due to its higher strength, superior formability, better wear resistance, and a resistance to weld cracking. 718Plus alloy is a lower cost option than Waspaloy or Rene 41 alloy due to its lower intrinsic raw materials cost and improved hot workability which provides higher material yields, resulting in a lower cost finished part.

Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base SuperalloyInconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy

Chemical composition

Element C Mn Si P S Cr Ni Mo Nb Ti Al Co W B Cu Pb Bi Se Fe
Weight(%) 0.01-0.05 0.35 max 0.35 max 0.004-0.020 0.0025 max 17.00-21.00 Rem 2.50-3.10 5.20-5.80 0.50-1.00 1.20-1.70 8.00-10.00 0.80-1.40 0.003-0.008 0.30 max 0.0005 max 0.00003 max 0.0003 max 8.00-10.00

Hardness

HRC 25 - 35(solution heat treated depending on quench rate)

HRC 42 - 48(fully aged condition)

Tensile Strength, Ultimate 1480 MPa

Application

These products have been typically used for parts requiring high resistance to creep and stress rupture up to 1400°F(760°C) and oxidation resistance up to 1800°F(982°C), but usage is not limited to such applications.

Available forms

718Plus alloy is available in all product forms: ingot, billet, block, forged round bar, hot-rolled shapes and rectangles, bar, rod, wire, plate, sheet, strip, and castings.

Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy


Product Tags:

N07818 nickel superalloy

      

AMS 5442 nickel superalloy

      

nickel base superalloy

      
Cheap Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy for sale

Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Suzhou Xunshi New Material Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)